EPOXY SYSTEMS
|
|
Epoxy resin Ε 481 EE: 175 Very resistant to crystallization at low temperatures Viscosity at 25o C (mPas) 600-750 Room temperature curing . Suitable for RTM and infusion
|
|
Epoxy resin Ε 476 EE: 195 Resistant to crystallization at low temperatures Viscosity at 25o C (mPas) 800-1000 Room temperature or elevated temperature curing
|
|
Epoxy resin Ε 447 EE: 200 Storing at temperatures above 25 o C Viscosity at 25o C (mPas) 600-800 Elevated temperature or room temperature curing .Very resistant to chemical attacks and acids |
|
Hardener H 17-20-12 HE: 34. Mixing ratio: 18 / 100 ( for 190 resin EE). Open time: 20’ at 25o C . Initial curing at 12 hours at 20o C. Peak exotherm of 150g at 25ο C: At 16 minutes 198ο C Πολύ καλός σε τήξη με χαμηλές θερμοκρασίες (<10οC).
|
|
Hardener H 20-40-18 HE: 38 Mixing ratio: 20 / 100 ( for 190 resin EE). Open time: 40’ at 25o C. Initial curing at 18 hours at 20o C. Peak exotherm of 150g at 25ο C: At 65 minutes 185ο C Εξαιρετικές μηχανικές ιδιότητες. καλός σε χαμηλές θερμοκρασίες
|
|
Hardener H 50-55-24 HE: 95 Mixing ratio: 50 / 100 ( for 190 resin EE). Open time: 55’ at 25o C. Initial curing at 24 hours at 20o C. Peak exotherm of 150g at 25ο C: At 50 minutes 140ο C Αντίσταση στο κιτρίνισμα. Μηχανικές ιδιότητες. Δυνατότητα επαφής με τρόφιμα.
|
|
Hardener H 58-65-36 HE: 114 Mixing ratio: 60 / 100 ( for 190 resin EE). Open time: 65’ at 25o C. Initial curing at 36 hours at 20o C. Peak exotherm of 150g at 25ο C: At 37 minutes 102ο C Αντίσταση στο κιτρίνισμα. Υψηλές χημικές αντιστάσεις. Δυνατότητα επαφής με τρόφιμα.
|

|
All FIBERMAX epoxy systems can be mixed. This way you can choose any combination of resin and hardener you like. In addition you have the capability of formulating a system that exactly meets your needs by mixing 2 or more hardeners or resins. FIBERMAX recommends precise mixing ratio of resin and hardener for optimum systems’ performance. |
|